ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It complies with FDA regulation 21 CFR 177.1520 (c) 3.1b. It is not to be used in packing or holding food during cooking. Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |