MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont 20 Series 20-6064 Specialty Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flexibility and environmental stress crack resistance and contains an antistatic agent.

Typical Applications: Injection blow molded closures where close thread tolerances are required; Ophthalmic solution containers; Other pharmaceutical and medical bottles and closures; Personal care containers and closures;

Features & Benefits: Superior resistance to environmental stress cracking; High flexibility; Good heat stability; Excellent color; Odor free; Excellent chemical resistance; Good mold release performance; Nontoxic; Antistatic agent reduces dust accumulation on store shelves.

Information provided by DuPont Packaging Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646ASTM D2240
Tensile Strength, Ultimate 14.4 MPa2090 psiASTM D638
Tensile Strength, Yield 9.60 MPa1390 psiASTM D638
Elongation at Break 540 %540 %ASTM D638
Modulus of Elasticity 0.186 GPa27.0 ksiASTM D638
Flexural Modulus 0.168 GPa24.4 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 0.430 J/cm
@Temperature -40.0 °C
0.806 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 94.0 °C201 °FFreezing Point via DSC/ASTM D3418
 109 °C228 °FUpon Melting via DSC/ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C111 °FASTM D648
Vicat Softening Point 94.0 °C201 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51ASTM D542
 
Processing PropertiesMetricEnglishComments
Processing Temperature 218 °C424 °FTypical Nozzle Ext. and Manifold temp for injection blow molding.
Nozzle Temperature 218 °C424 °FDie

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont 20 Series 2010 Specialty Polyethylene Resin
DuPont 20 Series DPE 20 Specialty Polyethylene Resin
DuPont 20 Series 2020T Specialty Polyethylene Resin
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade
Dow ATTANE™ 4206 Ultra Low Density Polyethylene, Impact Modifier Grade

PDUPF4 / 33601

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.