MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Armacell Ensolite™ EF0 EPDM crushed foam
Categories: Other Engineering Material; Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Super soft EPDM crushed (semi-closed cell) foam.
  • UL 94 5VA, V-0 HF-1 listed for flame
  • Meets Toyota TSK 6505F Class 2A
  • Manufactured in continuous rolls
  • Excellent resistance to ozone, weathering and heat
  • ASTM E-84 (25/50 Rated)

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0641 - 0.128 g/cc0.00231 - 0.00463 lb/in³ASTM D1056
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 0.00 - 100.00 - 10ASTM D2240
Tensile Strength >= 0.0689 MPa>= 10.0 psiASTM D412, Die A
Elongation at Break >= 125 %>= 125 %ASTM D412
Compressive Strength <= 0.00689 MPa
@Strain 25 %
<= 1.00 psi
@Strain 25 %
ASTM D1056
Tear Strength >= 0.701 kN/m>= 4.00 pliDie C; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FIntermittent; ASTM D1056
Minimum Service Temperature, Air -56.7 °C-70.0 °FASTM D1056
Flammability, UL94  V-0
@Thickness 3.15 - 3.40 mm
V-0
@Thickness 0.124 - 0.134 in
 5VA
@Thickness 4.29 - 4.72 mm
5VA
@Thickness 0.169 - 0.186 in
 
Descriptive Properties
Accelerated Aging±30%Change in Compression Deflection, 7 days at 70°C, ASTM D1056
FlammabilityHF-13.37-3.65 mm
 PassFMVSS-320, <'3.18 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Ensolite™ ECF-400 EPDM crushed foam
Ethylene Propylene Rubber (EPM, EPDM)
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding

PARMD062 / 186673

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.