MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: For best results, use low screw RPM.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D 792
Additive Loading 15 %15 %Primary Additive
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 838310 s delay; ASTM D 2240
Hardness, Shore D 3434instantaneous; ASTM D 2240
Tensile Strength at Break  4.83 MPa
@Thickness 3.20 mm
700 psi
@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 638
 17.9 MPa
@Thickness 3.20 mm
2600 psi
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 78.9 kN/m450 pliDie C; ASTM D 624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  56 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
56 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 57 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
57 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 58 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
58 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 59 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
59 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 61 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
61 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 63 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
63 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 232 °C380 - 450 °F
Mold Temperature 15.6 - 43.3 °C60.0 - 110 °F
Drying Temperature 93.3 °C
@Time 10800 - 21600 sec
200 °F
@Time 3.00 - 6.00 hour
Moisture Content <= 0.050 %<= 0.050 %
Dew Point -17.8 °C0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 2561 FR UV Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - UV Stabilized
RTP Company ESD 289 Nylon 6/6 (PA); Carbon Fiber - Electrically Conductive
RTP Company EMI 2562 UV BLACK Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company EMI 362 UV BLACK Polycarbonate (PC); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized

PQZRA37112 / 205877

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.