MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lotte Advanced Materials Infino® AE-2230 PC/PET, 20% MF
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Auto exterior applications

Information provided by Lotte Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccNatural or representative color; ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
20 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Ash 20 %20 %ASTM D5630
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength at Break 57.9 MPa8400 psi50 mm/min; ASTM D638
Tensile Strength, Yield 57.9 MPa8390 psi50 mm/min; ASTM D638
Elongation at Break 7.0 %7.0 %50 mm/min; ASTM D638
Tensile Modulus 3.73 GPa540 ksi50 mm/min; ASTM D638
Flexural Strength 76.5 MPa11100 psi2 mm/min; ASTM D790
Flexural Modulus 3.92 GPa569 ksi2 mm/min; ASTM D790
Izod Impact, Notched  0.490 J/cm
@Thickness 6.35 mm,
Temperature -30.0 °C
0.918 ft-lb/in
@Thickness 0.250 in,
Temperature -22.0 °F
ASTM D256
 0.490 J/cm
@Thickness 3.17 mm,
Temperature -30.0 °C
0.918 ft-lb/in
@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
 0.686 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.29 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 0.686 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.29 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
@Thickness 6.40 mm
266 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
@Thickness 6.40 mm
248 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 135 °C275 °FB/50; ISO R 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® AE-2150 PC/PET, 15% MF
MRC Polymers NAXALOY™ 793 PC/PET Blend, High Impact Strength and Chemical Resistance
Covestro Makroblend® AR205 PC+PET
Lotte Advanced Materials Infino® ASF-9810F PBT/PET/MF
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)

PLOTT9802 / 205665

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.