MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro Makroblend® AR205 PC+PET
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: (PC+PET) blend, easy flow, impact modified; application: automotive body panels

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183-1
Viscosity 200 cP
@Frequency 1000 Hz,
Temperature 270 °C
200 cP
@Frequency 1000 Hz,
Temperature 518 °F
b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in150x105x3 mm; 270 °C / MT 70°C; 600 bar; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in150x105x3 mm; 270 °C / MT 70°C; 600 bar; b.o. ISO 2577
Melt Flow 38 g/10 min
@Load 5.00 kg,
Temperature 270 °C
38 g/10 min
@Load 11.0 lb,
Temperature 518 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 45.0 MPa6530 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 4.8 %4.8 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.20 GPa319 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 80.0 MPa11600 psi2 mm/min; ISO 178
Flexural Yield Strength 68.0 MPa
@Strain 3.5 %
9860 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.20 GPa319 ksi2 mm/min; ISO 178
Flexural Strain at Yield 5.8 %5.8 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  20.0 kJ/m²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-1C
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180-1C
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
Impact  3900
@Temperature 23.0 °C
3900
@Temperature 73.4 °F
[N], Puncture Max Force; ISO 6603-2
 5000
@Temperature -30.0 °C
5000
@Temperature -22.0 °F
[N], Puncture Max Force; ISO 6603-2
Puncture Energy  42.0 J
@Temperature 23.0 °C
31.0 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 48.0 J
@Temperature -30.0 °C
35.4 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
45.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 82.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
45.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 126 °C259 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FISO 75-1,-2
Vicat Softening Point 138 °C
@Load 5.10 kg
280 °F
@Load 11.2 lb
120°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FISO 294
Mold Temperature 70.0 °C158 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® UT250 HR PC+PET
Covestro Makroblend® UT203 PC+PET
Covestro Makroblend® UT235 M PC+PET
Covestro Makroblend® M525 PC+PET
Covestro Makroblend® UT6007 PC+PBT

PCOVEST0797 / 202580

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.