MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Henkel Loctite® 3166 Deep Potting Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced; Epoxy, Thermally Conductive

Material Notes:
Potters
Loctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies.

For electronics assembly, Loctite offers deep potting, high adhesion, non-corrosive, and thermally conductive potting products. These can be cured with heat, UV light, or moisture.

Loctite® 3166 Deep Potting Epoxy
A heat cure soft epoxy for deep potting applications that require low shrinkage, thermal stability and environmental resistance. Cure Type: Heat Bonding Type: 2 part epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1800 cP1800 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1515
Hardness, Shore OO 6464
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg -27.0 °C-16.6 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min
@Temperature 80.0 °C
3.00 hour
@Temperature 176 °F
Pot Life 30.0 min
@Temperature 80.0 °C
30.0 min
@Temperature 176 °F
Gel Time 90.0 min90.0 minat 80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® 3180 Deep Potting Polyurethane
Elantas EN-2543 (Conap) Potting and Encapsulation Adhesive
Dymax 952 Potting and Encapsulation Adhesive
Dymax 3092P Fast Shallow Potting Compound and Sealant
Dymax 3069P Fast Shallow Potting Compound and Sealant

PLOCT195 / 51931

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.