General 7075 characteristics and uses (from Alcoa): Very high strength material used for highly stressed structural parts. The T7351 temper offers improved stress-corrosion cracking resistance. Uses: Aircraft fittings, gears and shafts, fuse parts, meter shafts and gears, missile parts, regulating valve parts, worm gears, keys, aircraft, aerospace and defense applications. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN. Composition Notes: A Zr + Ti limit of 0.25 percent maximum may be used with this alloy designation for extruded and forged products only, but only when the supplier and the purchaser have mutually agreed. Composition information provided by the Aluminum Association and is not for design. |
UNS A97075; ISO AlZn5.5MgCu(A); Aluminium 7075-O; AA7075-O; Al7075-O |