MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Escorene® LL-5002 LLDPE Compounding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Compounding Resin

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A linear low density polyethylene resin designed to provide good processability and ease of blending. LL-5002 also exhibits good toughness and environmental stress crack resistance.

Applications: Color concentrates; Slip and antiblock masterbatches.

Key Words: Linear Low Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³Exxon Method
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourF50, Igepal, Condition C; ASTM D1693
Melt Flow 2.0 g/10 min2.0 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ASTM D2240
Tensile Strength, Ultimate 21.0 MPa3050 psiASTM D638
Tensile Strength, Yield 10.0 MPa1450 psiASTM D638
Elongation at Break 800 %800 %
Flexural Modulus 0.218 GPa31.6 ksiASTM D790
Tensile Impact Strength 231 kJ/m²110 ft-lb/in²23°C; ASTM D-1822
Dart Drop, Total Energy 37.0 J
@Temperature -40.0 °C
27.3 ft-lb
@Temperature -40.0 °F
F50; ASTM D-3029
 
Thermal PropertiesMetricEnglishComments
Melting Point 121 °C250 °FExxon Method
Brittleness Temperature -70.0 °C-94.0 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating
LyondellBasell Petrothene® NA217080 Low Density Polyethylene
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene
LG Chemical LUTENE LB4500 LDPE Extrusion Coating
ExxonMobil LD 202.48 Extrusion Coating Resin

PEXCGH / 37965

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.