System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
;
Low Density Polyethylene (LDPE), Extrusion Grade
Material Notes:
LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.
Application examples: coating of paper, paperboard, aluminum.
Information provided by Total Petrochemicals.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.924
g/cc
0.924
g/cc
ISO 1183
Melt Flow
4.0
g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
13.0
MPa
1890
psi
ISO 527-2
Tensile Strength, Yield
11.0
MPa
1600
psi
ISO 527-2
Elongation at Break
550 %
550 %
ISO 527-2
Modulus of Elasticity
0.250
GPa
36.3
ksi
ISO 527-2
Thermal Properties
Metric
English
Comments
Melting Point
111
°C
232
°F
ISO 11357
Vicat Softening Point
95.0
°C
203
°F
ISO 306
Processing Properties
Metric
English
Comments
Processing Temperature
200
-
320
°C
392
-
608
°F
Melt Temperature
260
-
320
°C
500
-
608
°F
Die Melt Temp
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
Dow LDPE 4005 Low Density Polyethylene, Extrusion Coating Grade
ExxonMobil LD 202.48 Extrusion Coating Resin
PTOTAL716 / 130441
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.