MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt Silvaloy® 250 Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Braze 250 is an intermediate temperature silver brazing alloy with a long (325EF/180EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through its melting range. Therefore, it is preferable to use this alloy where the assembly can be heated rapidly to brazing temperature. The long melting range of this alloy is useful when wide gap joints are brazed since it assists in producing larger fillets than more fluid alloys. Where the higher brazing temperature and characteristics of this alloy are permissible, the lower silver content affords a saving.

Applications:Braze 250 is a useful intermediate temperature brazing alloy for joining a variety of ferrous and non-ferrous alloys capable of being heated to 1600EF/870EC without damage. It has found special use as a bearing surface material on rubbing seals in jet engine compressors.

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.95 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 172 - 207 MPa25000 - 30000 psiCopper butt joint
 241 - 276 MPa35000 - 40000 psiNickel-Silver butt joint
 241 - 310 MPa35000 - 45000 psiBrass butt joint
Elongation at Break 8.0 - 9.0 %8.0 - 9.0 %% in 2", Copper butt joint
 9.0 - 18 %9.0 - 18 %% in 2", Brass butt joint
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000706 ohm-cm0.00000706 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 677 - 857.2 °C1250 - 1575 °F
Solidus 677 °C1250 °FMelting Point
Liquidus 857.2 °C1575 °FFlow Point
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 51.5 - 53.5 %51.5 - 53.5 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 24 - 26 %24 - 26 %
Zinc, Zn 21.5 - 23.5 %21.5 - 23.5 %
 
Descriptive Properties
ColorBrass Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Overview of materials for Silver Alloy
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt Silvaloy® A20 Brazing Alloy
Johnson Matthey Infil-bond™ 30Ag Infiltrant/Binder Product

NLUCMI19 / 18086

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.