MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy; Pure Element

Material Notes: Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and rupture discs. Fine silver is generally selected for its high thermal and electrical conductivity, as well as for its good resistance to oxidation and corrosive attack. It also exhibits excellent ductility and is easily joined by welding or brazing.

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.49 g/cc0.3790 lb/in³
Vapor Pressure 0.00133 bar
@Temperature 1360 °C
1.00 torr
@Temperature 2480 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 107.87107.87
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 - 207 MPa24000 - 30000 psiWire, Temper-Soft
 165 - 207 MPa24000 - 30000 psiStrip, Temper-Soft
 179 - 228 MPa26000 - 33000 psiStrip, Temper-1/4 Hard
 207 - 255 MPa30000 - 37000 psiStrip, Temper-1/2 Hard
 207 - 255 MPa30000 - 37000 psiWire, Temper- 1/4 Hard
 255 - 303 MPa37000 - 44000 psiStrip, Temper-Hard
 269 - 317 MPa39000 - 46000 psiWire, Temper- 1/2 Hard
 283 - 324 MPa41000 - 47000 psiStrip, Temper-Ex. Hard
 290 - 338 MPa42000 - 49000 psiWire, Temper- Hard
 303 - 352 MPa44000 - 51000 psiStrip, Temper-Spring
 317 - 365 MPa46000 - 53000 psiWire, Temper-Ex. Hard
 324 - 372 MPa47000 - 54000 psiWire, Temper-Spring
 331 - 379 MPa48000 - 55000 psiStrip, Temper-Ex. Spring
 331 - 379 MPa48000 - 55000 psiWire, Temper-Ex. Spring
Elongation at Break >= 1.0 %>= 1.0 %% in 2", Strip, Temper-Spring
 >= 1.0 %>= 1.0 %% in 2", Strip, Temper-Ex. Spring
 >= 1.0 %>= 1.0 %% in 2", Wire, Temper-Spring
 >= 1.0 %>= 1.0 %% in 2", Wire, Temper- Ex. Spring
 >= 2.0 %>= 2.0 %% in 2", Strip, Temper-Ex. Hard
 >= 2.0 %>= 2.0 %% in 2", Wire, Temper- Hard
 >= 2.0 %>= 2.0 %% in 2", Wire, Temper- Ex. Hard
 >= 3.0 %>= 3.0 %% in 2", Strip, Temper- Hard
 >= 4.0 %>= 4.0 %% in 2", Wire, Temper- 1/4 Hard
 >= 4.0 %>= 4.0 %% in 2", Wire, Temper- 1/2 Hard
 >= 8.0 %>= 8.0 %% in 2", Strip, Temper-1/2 Hard
 >= 18 %>= 18 %% in 2", Strip, Temper- 1/4 Hard
 >= 25 %>= 25 %% in 2", Strip, Temper-Soft
 >= 25 %>= 25 %% in 2", Wire, Temper-Soft
Reduction of Area 0.00 %0.00 %Strip, Temper-Soft
 0.00 %0.00 %Wire, Temper-Soft
 11 %11 %Strip, Temper-1/4 Hard
 21 %21 %Strip, Temper-1/2 Hard
 21 %21 %Wire, Temper-1/4 Hard
 37 %37 %Wire, Temper-1/2 Hard
 37 %37 %Strip, Temper-Hard
 50 %50 %Strip, Temper- Ex. Hard
 60 %60 %Strip, Temper-Spring
 60 %60 %Wire, Temper- Hard
 69 %69 %Strip Temper, Ex. Spring
 75 %75 %Wire, Temper-Ex. Hard
 84 %84 %Wire, Temper-Spring
 90 %90 %Wire, Temper-Ex. Spring
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000001642 ohm-cm
@Temperature 20.0 °C
0.000001642 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C
@Temperature 0.000 - 100 °C
10.6 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.2343 J/g-°C
@Temperature 20.0 °C
0.05600 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 418 W/m-K
@Temperature 20.0 °C
2900 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 960.8 °C1761 °F
Boiling Point 2210 °C4010 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0020 %<= 0.0020 %
Bismuth, Bi <= 0.0010 %<= 0.0010 %
Cadmium, Cd <= 0.0050 %<= 0.0050 %
Copper, Cu <= 0.080 %<= 0.080 %
Iron, Fe <= 0.0050 %<= 0.0050 %
Lead, Pb <= 0.025 %<= 0.025 %
Nickel, Ni <= 0.0020 %<= 0.0020 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag >= 99.95 %>= 99.95 %
Zinc, Zn <= 0.0050 %<= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silver Alloy
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt Silvaloy® A20 Brazing Alloy
Cadi 50WS Tungsten Silver
Lucas-Milhaupt Silvaloy® 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal

NLUCMI39 / 18106

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.