MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik VESTAMID® EX9203 black Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: Medium-viscosity, halogen-free flame-retardant polyamide 12 compound. VESTAMID® EX9203 black is a medium viscosity, heat-stabilized polyamide 12 and is prepared with an efficient halogen-free flame retardant. VESTAMID® EX9203 black has been developed especially for the extrusion of corrugated tubes and is distinguished by the following characteristics: high impact strength and flexibility, also at low temperatures, especially good flexural fatigue behavior softening by non-migrating polyamide elastomer, good dimensional stability and constant mechanical properties at changing ambient humidity due to low water absorption of polyamide 12, good chemical resistance, good ageing stability. Because of the halogen-free flame retardant the mold temperature should preferably be within a range of 210°C to 230°C, but not higher than 240°C. VESTAMID® EX9203 black is supplied as cylindrical granules, ready for processing in moisture-proof packaging.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Water Absorption 0.010 %0.010 %Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.0 MPa4060 psiISO 527
Tensile Strength, Yield 24.0 MPa3480 psiISO 527
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527
 245 %245 %ISO 527
Elongation at Yield 14 %14 %ISO 527
Tensile Modulus 0.760 GPa110 ksiISO 527
50% Modulus 22.0 MPa
@Strain 50 %
22.0 MPa
@Strain 50 %
ISO 527
Charpy Impact, Notched  0.410 J/cm²
@Temperature -30.0 °C
1.95 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 177 °C351 °FISO 11357-1/-3
Flammability Test 3.0
@Thickness 0.800 mm
3.0
@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 30 %30 %ISO 4589-1/-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® LX9112 Nylon 12
Ashley Polymers Ashlene® TD930H Nylon 12
Evonik VESTAMID® LX9102 PA 12
Evonik VESTAMID® LX9110 black | PA12 Nylon 12
LATI Latamid 12 CP/85 PA 12

PEVONIK833 / 243042

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.