Standard injection molding grade, easy flow, easy mold release, fast setting. Applications: Thin walled engineering parts. Automotive sector: air filters, switch and connector parts for car electric. Electrical sector: switch and connector parts Triax® is now a INEOS Styrolution trade name; this grade is discontinued. Information provided by the manufacturer. |