MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Elix Polymers ELIX™ 152 I Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: High rubber content ABS copolymer used for polymers modification purposes.

Typical Applications:

  • Modifier for improving process ability (extrusion, thermoforming, calendering operations), thermal resistance, tensile and impact strength of opaque PVC compounds; typical applications include profiles, semi-rigid sheets, decorative films (furniture, automotive interior trim) and injection molded parts
  • Used to improve toughness of PC-based blends, SAN copolymers and SMA resins
  • Cost-effective product applied to increase TPU performance
Chemical composition: Acrylonitrile-Butadiene-Styrene Copolymer

Physical form: White to slightly yellow powder

Information provided by Elix Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.280 - 0.370 g/cc0.0101 - 0.0134 lb/in³
Maximum Moisture Content 1.21.2
 
Descriptive Properties
Content<0.2%Residual monomers
 51-54%Polybutadiene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GEHR Plastics ABS Acrylonitrile Butadiene Styrene
Denka MALECCA K-090 ABS
Ineos ABS Lustran® 723-1, Extrusion Grade
Omnia Plastica ABS Acrylonitrile-butadiene-styrene
Chase Plastics CP Pryme® A100HF ABS

PELIX037 / 183352

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.