MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Envalior TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 50% Glass Fiber Filler

Material Notes: Within the TEPEX® composite laminate, PP is a resin known for its good hardness, stiffness, abrasion resistance and chemical resistance.
Typical application environments are within automotive applications, large structural parts.

Former Lanxess (Bond Lamiantes Division) product line is now with Envalior.'

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³
Filler Content 47 %47 %by volume
Thickness 500 microns19.7 millaminate layer thickness
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 390 MPa56600 psitransverse; ISO 527-4/5
 400 MPa58000 psilongitudinal; ISO 527-4/5
Tensile Modulus 20.1 GPa2920 ksitransverse; ISO 527-4/5
 20.5 GPa2970 ksilongitudinal; ISO 527-4/5
Flexural Strength 365 MPa52900 psitransverse; ISO 178
 370 MPa53700 psilongitudinal; ISO 178
Flexural Modulus 17.0 GPa2470 ksitransverse; ISO 178
 17.5 GPa2540 ksilongitudinal; ISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FDSC 3146
Maximum Service Temperature, Air 90.0 °C
@Time 7.20e+7 sec
194 °F
@Time 20000 hour
Relative Temperature Index; IEC 216/1
Deflection Temperature at 1.8 MPa (264 psi) 158 °C316 °FISO 75-1/2
Minimum Service Temperature, Air -10.0 °C14.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 210 °C374 - 410 °F
 
Descriptive Properties
ReinforcementArea weight600 g/m²
 Fabrictwill 2/2
 Fibersroving glass
 Weight Rate50% longitudinal and transverse
 Yarn1200 tex longitudinal and transverse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate

PBONDL983 / 140566

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.