MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Carbon Fiber Filled

Material Notes: Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is aerospace qualified. This material has outstanding mechanical properties and fatigue resistance.
Typical application environments are structural sporting goods applications, helmet shells.

Former Lanxess (Bond Lamiantes Division) product line is now with Envalior.'

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³
Filler Content 45 %45 %by volume
Thickness 250 microns9.84 millaminate layer thickness
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 725 MPa105000 psitransverse; ISO 527-4/5
 785 MPa114000 psilongitudinal; ISO 527-4/5
Elongation at Break 2.1 %2.1 %longitudinal; ISO 527-4/5
 2.1 %2.1 %transverse; ISO 527-4/5
Tensile Modulus 51.0 GPa7400 ksitransverse; ISO 527-4/5
 53.0 GPa7690 ksilongitudinal; ISO 527-4/5
Flexural Strength 730 MPa106000 psitransverse; ISO 178
 760 MPa110000 psilongitudinal; ISO 178
Flexural Modulus 44.1 GPa6400 ksitransverse; ISO 178
 45.5 GPa6600 ksilongitudinal; ISO 178
Poissons Ratio 0.0700.070longitudinal; ISO 527-4/5
 0.0700.070transverse; ISO 527-4/5
Charpy Impact Unnotched  11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
longitudinal; ISO 179/1eU
 15.0 J/cm²
@Temperature -30.0 °C
71.4 ft-lb/in²
@Temperature -22.0 °F
longitudinal; ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDSC 3146
Maximum Service Temperature, Air 130 °C
@Time 7.20e+7 sec
266 °F
@Time 20000 hour
Relative Temperature Index; IEC 216/1
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75-1/2
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Glass Transition Temp, Tg 70.0 °C158 °FDSC 3146
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 - 300 °C536 - 572 °F
 
Descriptive Properties
ReinforcementArea weight200 g/m²
 Fabrictwill 2/2
 Fiberscarbon
 Weight Rate50% longitudinal and transverse
 Yarn3000 tex longitudinal and transverse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 408-C200(2)-FG290(2)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate

PBONDL987 / 140570

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.