MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Overview of materials for Ethylene Butyl Acrylate
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.895 - 1.48 g/cc0.0323 - 0.0535 lb/in³Average value: 0.979 g/cc Grade Count:109
Viscosity 8300 - 8340 cP
@Temperature 190 - 190 °C
8300 - 8340 cP
@Temperature 374 - 374 °F
Average value: 8320 cP Grade Count:2
Butyl Acrylate Content 3.00 - 37.0 %3.00 - 37.0 %Average value: 21.4 % Grade Count:25
Thickness 25.0 - 40.0 microns0.984 - 1.57 milAverage value: 35.0 microns Grade Count:3
Melt Flow 0.250 - 900 g/10 min0.250 - 900 g/10 minAverage value: 36.7 g/10 min Grade Count:108
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40.0 - 97.040.0 - 97.0Average value: 73.6 Grade Count:32
Hardness, Shore D 23.0 - 80.023.0 - 80.0Average value: 41.2 Grade Count:26
Tensile Strength, Ultimate 0.965 - 31.0 MPa140 - 4500 psiAverage value: 13.4 MPa Grade Count:72
Tensile Strength, Yield 3.50 - 38.0 MPa508 - 5510 psiAverage value: 20.9 MPa Grade Count:64
Film Elongation at Break, MD 200 - 830 %200 - 830 %Average value: 563 % Grade Count:11
Film Elongation at Break, TD 600 - 850 %600 - 850 %Average value: 708 % Grade Count:11
Elongation at Break 4.00 - 1210 %4.00 - 1210 %Average value: 326 % Grade Count:76
Elongation at Yield 2.30 - 14.5 %2.30 - 14.5 %Average value: 5.52 % Grade Count:42
Modulus of Elasticity 0.0250 - 4.50 GPa3.63 - 653 ksiAverage value: 1.66 GPa Grade Count:46
Flexural Modulus 0.00538 - 4.35 GPa0.780 - 631 ksiAverage value: 1.37 GPa Grade Count:38
Izod Impact Unnotched 4.20304 - 4.20304 J
@Temperature -17.8 - -17.8 °C
3.10000 - 3.10000 ft-lb
@Temperature 0.000 - 0.000 °F
Average value: 4.20 J Grade Count:1
Izod Impact, Notched (ISO) 3.15 - 52.5 kJ/m²1.50 - 25.0 ft-lb/in²Average value: 34.3 kJ/m² Grade Count:7
Charpy Impact Unnotched 2.31 - 10.1 J/cm²11.0 - 48.0 ft-lb/in²Average value: 5.32 J/cm² Grade Count:3
 1.596 - 2.10 J/cm²
@Temperature -30.0 - 0.000 °C
7.596 - 9.99 ft-lb/in²
@Temperature -22.0 - 32.0 °F
Average value: 1.85 J/cm² Grade Count:1
Charpy Impact, Notched 0.231 - 6.51 J/cm²1.10 - 31.0 ft-lb/in²Average value: 1.42 J/cm² Grade Count:38
 0.1302 - 1.491 J/cm²
@Temperature -30.0 - 0.000 °C
0.6197 - 7.096 ft-lb/in²
@Temperature -22.0 - 32.0 °F
Average value: 0.606 J/cm² Grade Count:28
Gardner Impact  8.83543 - 8.83543 J
@Temperature -28.9 - -28.9 °C
6.51667 - 6.51667 ft-lb
@Temperature -20.0 - -20.0 °F
Average value: 8.84 J Grade Count:1
 8.83543 - 8.83543 J
@Thickness 3.17 - 3.17 mm
6.51667 - 6.51667 ft-lb
@Thickness 0.125 - 0.125 in
Average value: 8.84 J Grade Count:1
Dart Drop, Total Energy 24.9471 - 29.0145 J
@Temperature -30.0 - -15.0 °C
18.4000 - 21.4000 ft-lb
@Temperature -22.0 - 5.00 °F
Average value: 26.3 J Grade Count:5
 26.1673 - 26.1673 J
@Temperature -30.0 - -30.0 °C
19.3000 - 19.3000 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 26.3 J Grade Count:1
 26.1673 - 26.1673 J
@Thickness 3.20 - 3.20 mm
19.3000 - 19.3000 ft-lb
@Thickness 0.126 - 0.126 in
Average value: 26.3 J Grade Count:1
Coefficient of Friction 0.100 - 1.300.100 - 1.30Average value: 0.500 Grade Count:4
Elmendorf Tear Strength MD 367 - 1270 g367 - 1270 gAverage value: 679 g Grade Count:3
Elmendorf Tear Strength TD 399 - 1360 g399 - 1360 gAverage value: 783 g Grade Count:3
Dart Drop Test 600 - 1500 g1.32 - 3.31 lbAverage value: 1170 g Grade Count:3
Film Tensile Strength at Break, MD 20.0 - 29.0 MPa2900 - 4210 psiAverage value: 24.6 MPa Grade Count:7
Film Tensile Strength at Break, TD 15.0 - 30.0 MPa2180 - 4350 psiAverage value: 22.0 MPa Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 25.0 - 1.00e+16 ohm-cm25.0 - 1.00e+16 ohm-cmAverage value: 2.95e+15 ohm-cm Grade Count:4
 40.0 - 3.60e+14 ohm-cm
@Temperature 70.0 - 90.0 °C
40.0 - 3.60e+14 ohm-cm
@Temperature 158 - 194 °F
Average value: 1.90e+14 ohm-cm Grade Count:3
Surface Resistance 1.70e+14 - 4.80e+14 ohm
@Temperature 70.0 - 70.0 °C
1.70e+14 - 4.80e+14 ohm
@Temperature 158 - 158 °F
Average value: 3.25e+14 ohm Grade Count:2
Dielectric Constant 2.70 - 6.102.70 - 6.10Average value: 4.28 Grade Count:3
Dissipation Factor 0.00100 - 0.1330.00100 - 0.133Average value: 0.0462 Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.4 - 77.4 µm/m-°C28.0 - 43.0 µin/in-°FAverage value: 58.3 µm/m-°C Grade Count:5
Melting Point 59.0 - 285 °C138 - 545 °FAverage value: 92.3 °C Grade Count:50
Deflection Temperature at 0.46 MPa (66 psi) 68.9 - 142 °C156 - 288 °FAverage value: 104 °C Grade Count:30
Deflection Temperature at 1.8 MPa (264 psi) 43.9 - 92.8 °C111 - 199 °FAverage value: 57.1 °C Grade Count:47
Vicat Softening Point 40.0 - 153 °C104 - 307 °FAverage value: 63.8 °C Grade Count:25
Brittleness Temperature -73.0 - -30.0 °C-99.4 - -22.0 °FAverage value: -64.4 °C Grade Count:5
Glass Transition Temp, Tg -55.0 - -50.0 °C-67.0 - -58.0 °FAverage value: -53.9 °C Grade Count:9
Ring & Ball Softening Point 55.0 - 190 °C131 - 374 °FAverage value: 103 °C Grade Count:7
 
Optical PropertiesMetricEnglishComments
Haze 10.0 - 16.0 %10.0 - 16.0 %Average value: 14.0 % Grade Count:3
Gloss 60.0 - 70.0 %60.0 - 70.0 %Average value: 63.3 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 300 °C320 - 572 °FAverage value: 221 °C Grade Count:12
Adapter Temperature 180 - 290 °C356 - 554 °FAverage value: 240 °C Grade Count:6
Die Temperature 141 - 290 °C285 - 554 °FAverage value: 235 °C Grade Count:7
Melt Temperature 115 - 290 °C239 - 554 °FAverage value: 190 °C Grade Count:19

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvaloy® PTW Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade

O4170 / 77787

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.