MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 - 0.944 g/cc0.0335 - 0.0341 lb/in³Average value: 0.936 g/cc Grade Count:11
Viscosity  500000 - 900000 cP
@Temperature 190 - 190 °C
500000 - 900000 cP
@Temperature 374 - 374 °F
Average value: 700000 cP Grade Count:3
 500000 - 900000 cP
@Shear Rate 50.0 - 50.0 1/s
500000 - 900000 cP
@Shear Rate 50.0 - 50.0 1/s
Average value: 700000 cP Grade Count:3
Environmental Stress Crack Resistance >= 360 hour
@Temperature 50.0 - 50.0 °C
>= 360 hour
@Temperature 122 - 122 °F
Average value: 360 hour Grade Count:1
Methyl Acrylate Content 18.0 - 24.0 %18.0 - 24.0 %Average value: 21.7 % Grade Count:3
Melt Flow 2.00 - 13.5 g/10 min2.00 - 13.5 g/10 minAverage value: 7.70 g/10 min Grade Count:14
 
Mechanical PropertiesMetricEnglishComments
Seal Strength 1300 - 2800 g/25 mm1300 - 2800 g/inAverage value: 1960 g/25 mm Grade Count:5
Hot Tack Strength 500 - 2000 g/25 mm500 - 2000 g/inAverage value: 1030 g/25 mm Grade Count:8
 
Thermal PropertiesMetricEnglishComments
Melting Point 60.0 - 109 °C140 - 228 °FAverage value: 86.5 °C Grade Count:14
Vicat Softening Point 45.6 - 90.0 °C114 - 194 °FAverage value: 70.5 °C Grade Count:14
 
Processing PropertiesMetricEnglishComments
Processing Temperature 154 - 315 °C309 - 599 °FAverage value: 238 °C Grade Count:4
Nozzle Temperature 230 - 305 °C446 - 581 °FAverage value: 279 °C Grade Count:10
Melt Temperature 220 - 315 °C428 - 599 °FAverage value: 278 °C Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
Overview of materials for Ethylene Butyl Acrylate
Arkema LOTRYL® 15 MA 03 Copolymer Ethylene - Methyl Acrylate

O4189 / 78301

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.