MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Chemical Advanced Materials Ketron™ LSG CC PEEK Ketron PEEK with 57% Woven Carbon Fiber  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: Life Science Grade, Polyetheretherketone
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc
@Temperature 22.8 °C
1.52 g/cc
@Temperature 73.0 °F
Water Absorption 0.018 %0.018 %IMMERSION; 24HRS; ASTM D570 2
Water Absorption at Saturation 0.053 %0.053 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 116116ASTM D785
Hardness, Shore D 94
@Temperature 22.8 °C
94
@Temperature 73.0 °F
ASTM D2240
Tensile Strength 586 MPa
@Temperature 22.8 °C
85000 psi
@Temperature 73.0 °F
ASTM D3039
Elongation at Break 1.6 %1.6 %ASTM D3039
Tensile Modulus 56.5 GPa
@Temperature 22.8 °C
8200 ksi
@Temperature 73.0 °F
ASTM D3039
Flexural Strength 793 MPa
@Temperature 22.8 °C
115000 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 51.7 GPa
@Temperature 22.8 °C
7500 ksi
@Temperature 73.0 °F
ASTM D790
Compressive Strength  586 MPa
@Temperature 22.8 °C
85000 psi
@Temperature 73.0 °F
z-direct (through plies); ASTM D695
 752 MPa
@Temperature 22.8 °C
109000 psi
@Temperature 73.0 °F
in-plane (across plies); ASTM D695
Compressive Modulus  8.96 GPa
@Temperature 22.8 °C
1300 ksi
@Temperature 73.0 °F
in-plane (across plies); ASTM D695
 29.0 GPa
@Temperature 22.8 °C
4200 ksi
@Temperature 73.0 °F
z-direct (through plies); ASTM D695
Izod Impact, Notched 4.70 J/cm
@Temperature 73.0 °C
8.80 ft-lb/in
@Temperature 163 °F
ASTM D256 Type A
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmEOS/ESD S11.11
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C650 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 304 °C580 °FASTM D648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ LSG CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone

P1SM18E / 171663

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.