MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Envalior TEPEX® dynalite 408-C200(2)-FG290(4)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Carbon Fiber Reinforced

Material Notes: Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and fatigue behavior and is easy to mold, obtaining an excellent surface quality. The TPU-carbon-glass laminates can easily be bonded with common adhesive systems. An excellent adhesion is achieved when overmolding with injection molding TPU grades.
Typical application environments are within automotive applications, large structural parts, bumper systems, structural sporting goods applications, helmet shells.

Former Lanxess (Bond Lamiantes Division) product line is now with Envalior.'

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³
Filler Content 45 %45 %by volume
Thickness 1500 microns59.1 millaminate layer thickness
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 630 MPa91400 psitransverse; ISO 178
 640 MPa92800 psilongitudinal; ISO 178
Flexural Modulus 35.0 GPa5080 ksitransverse; ISO 178
 35.5 GPa5150 ksilongitudinal; ISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 190 °C374 °FDSC 3146
Maximum Service Temperature, Air 90.0 °C
@Time 7.20e+7 sec
194 °F
@Time 20000 hour
Relative Temperature Index; IEC 216/1
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FISO 75-1/2
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 230 °C410 - 446 °F
 
Descriptive Properties
ReinforcementArea weight200 and 290 g/m²
 Fabrictwill 2/2
 Fiberscarbon and filament glass
 Weight Rate50% longitudinal and transverse
 Yarn3000/3x68 tex longitudinal and transverse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 408-C200(2)-FG290(2)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate

PBONDL990 / 140573

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.