MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Master Bond EP62-1LPSPMed Two component, high performance epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Exceptionally low viscosity
  • Very long open time at room temperature
  • Passes USP Class VI and ISO 10993-5 requirements
  • Capable of resisting repeated sterilization
Master Bond EP62-1LPSPMed is an ultra low viscosity, two part epoxy that passes biocompatibility testing. It has a forgiving mix ratio of 100 to 25 by weight. Upon mixing, the viscosity is markedly low and the working life is impressively long, 12-24 hours at room temperature. There are many curing options for EP62-1LPSPMed. The basic cure starts at room temperature overnight, followed by 3 options involving heat. First is heating for 8-10 hours at 60-70°C. Other options include 60-90 minutes at 80-100°C or 30-60 minutes at 125°C. Post curing at 100-150°C for 3-4 hours will help optimize properties. EP62-1LPSPMed blends an array of attractive physical strength properties and reliable electrical insulation values. It bonds well to a wide variety of substrates including metals, composites, glass and many plastics. It is cryogenically serviceable and has good heat resistance, with a temperature range extending from 4K to +400°F. EP62-1LPSPMed offers superior resistance to EtO, radiation, chemical sterilization media and autoclaving. It can be used for both reusable and disposable medical devices. In very thin sections, this system will transmit light, but in thicker ones, it is opaque. Also, its low viscosity makes it useful for smaller potting and encapsulating applications. An extra benefit of using EP62-1LPSPMed, is that the system has good toughness. This translates to enhanced ability to withstand thermal cycling, mechanical shock and vibration. The product property profile, especially its low viscosity and long working life, make it a very special type of biocompatible epoxy for medical device applications.

Product Advantages:

  • Easy to use, very forgiving 100 to 25 mix ratio by weight
  • Extremely low viscosity and very long working life
  • Superior resistance to a wide variety of sterilants
  • Excellent toughness, will resist thermal cycling
  • Highly useful electrical insulation properties
  • Cryogenically serviceable

Information provided by Masterbond.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Hardness, Shore D, After Aging; 85% RH
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, lap shear, Al/Al
  • Volume Resistivity
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time
  • Cure Time
  • Cure Time, Post cure for optimum properties
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, In original unopened containers
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.