MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Kolon KocetalĀ® K300 General Purpose Grade Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of products of Kocetal are short term: 140-150C and long term: 100-120C.

Mechanical Properties: Kocetal is an engineering plastic that has excellent strength, stiffness and wear endurance. Also, it offers an excellent balance of several properties. For example, mechanical properties are stable in the practical temperature zone (-50C to 80C), compared to Nylon and PBT resins. Although it has slightly lower initial strength, compared to homopolymer, the long term properties of "elongation at break and impact strength" are superior.

Electrical Properties: Kocetal has excellent electrical properties. Its electrical properties, volume resistivity, dielectric constant, dissipation factor and dielectric strength change little with temperature. It also has a feature of good anti-pollution properties on electrical contact. Kocetal has such a permanent anti-static grade that can be applied to the specifics.

Chemical Properties: Kocetal has excellent chemical resistance to organic chemicals, oils, fats and detergents. It is also strongly resistant to inorganic chemicals except strong acids.

Information provided by US distributor, API-Kolon.

Vendors:
Available Properties
  • Density, ASTM D790
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, ASTM D955
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, Ultimate, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Yield Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, ASTM D1894
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • CTE, linear, ASTM D696
  • Melting Point, ASTM D1525
  • Maximum Service Temperature, Air, Long Term
  • Maximum Service Temperature, Air, Short Term
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Flammability, UL94
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature, Surface
  • Drying Temperature
  • Dry Time
  • Injection Pressure
  • Screw Speed, Purge with polyethylene/polystyrene
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.