MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Borealis RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of the excellent performance characteristics of RA7050-GN is, for example, a categorized required strength (CRS) of 5 MPa at 70°C and 50 years in comparison to a value of 3.21 MPa for standard PP-R. RA7050 is steel grey similar to RAL7042.

RA7050-GN is intended to be used in applications for plumbing and heating, such as in-house hot and cold water pipes and fittings, floor and wall heating systems and radiator connections.

Former trade name for this product was Beta(ß)-PPR.

Information provided by the Manufacturer.

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527-2, At 50 mm/min
  • Elongation at Yield, ISO 527-2, At 50 mm/min
  • Modulus of Elasticity, ISO 527, 1 mm/min
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Surface Resistance, DIN 53482/VDE 0303 Part 2
  • Thermal Conductivity, DIN 52612 Part 1
  • Front Barrel Temperature
  • Die Temperature
  • Melt Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.