MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • EU and China RoHS compliant.
Applications:
  • Automotive-Air Induction System Ducts, Boots and Bellows for Steering and Suspension, Plugs, Bumpers, Grommets, Clips, Seals, Gaskets and Weather Seals
  • Consumer-Electronic and Floor Care
  • Industrial – Seals and Gaskets
  • Tubing
Uses:
  • Appliance Components
  • Consumer Applications
  • Gaskets
  • Automotive Applications
  • Diaphrams
  • Seals
  • Automotive Under the Hood
  • Electrical Parts
  • Tubing
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL JMLU2; UL QMFZ2; UL QMFZ8
Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Shore A, ISO 868, 2 mm, 15 sec
  • Hardness, Shore A, ASTM D573, Air at 302°F, 168 hr
  • Tensile Strength at Break, ASTM D573, Air at 302°F, 168 hr
  • Tensile Strength at Break, ASTM D412, Across Flow
  • Tensile Stress at Strain, ASTM D412
  • Elongation at Break, ASTM D573, Air at 302°F, 168 hr
  • Elongation at Break, ASTM D412, Across Flow
  • Tear Strength, ASTM D624, 73°C, Die C
  • Compression Set, ASTM D395
  • Compression Set, ASTM D395
  • Dielectric Constant, ASTM D150, 1.98 mm
  • Dielectric Strength, ASTM D149, 2.03 mm
  • Maximum Service Temperature, Air
  • Brittleness Temperature, ASTM D746
  • UL RTI, Electrical, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94
  • Processing Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Die Temperature, Extrusion
  • Melt Temperature, Extrusion
  • Melt Temperature, Processing
  • Mold Temperature, Processing
  • Drying Temperature
  • Dry Time
  • Moisture Content
  • Back Pressure, Processing
  • Back Pressure, Extrusion
  • Clamp Pressure
  • Vent Depth
  • Cushion
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.