MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Gougeon Brothers PRO-SET® ADV-175/ADV-276 Toughened Adhesive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Shear thinning resins and hardeners are thixotropic gels. The mixture fills gaps and will not sag on vertical surfaces. The material wets out the substrate, making priming or pre-wetting unnecessary on most surfaces, while ensuring a good bond.
Medium cure speed hardener provides approximately 50 minutes of working time at 72°F (22°C).
Room temperature cure properties suitable for many composite components and structures.
High performance pre-thickened, two-part epoxy adhesive delivers toughness and superior peel strength for heavily loaded applications and difficult to bond substrates including pre-preg, SMC, metals and most plastics. Also for secondary bonding of laminated composites, steel, aluminum, cast iron, concrete, stone, and most wood species. PRO-SET Adhesives bonds these material in any combination.
Coverage one cartridge set dispenses approximately 47' of 1/4" bead, or 17' of 1/2" bead and will cover approximately 7 sq ft when spread with a 1/8" x 1/8" notched spreader, or 12 sq ft with a 1/16" x 1/16" notched spreader.

Information provided by Gougeon Brothers, Inc.

Vendors:
Available Properties
  • Density, Hardener
  • Density, Cured
  • Density, Resin
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Shear Strength, ASTM D1002, on 1018 Steel
  • Shear Strength, ASTM D1002, on 2024T Aluminum
  • Adhesive Bond Strength, ASTM D4541, to 2024T Aluminum
  • Adhesive Bond Strength, ASTM D4541, to 1018 Steel
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Glass Transition Temp, Tg, ASTM E1356, DSC Onset– 1st Heat, Post cure 2 weeks at 22°C
  • Glass Transition Temp, Tg, ASTM E1356, DSC Onset– 1st Heat, Post cure 24 hrs at 38°C
  • Glass Transition Temp, Tg, ASTM E1356, DSC Onset– 1st Heat, Post cure 8 hrs at 60°C
  • Glass Transition Temp, Tg, ASTM E1356, DSC Onset– 1st Heat, Post cure 8 hrs at 82°C
  • Glass Transition Temp, Tg, ASTM E1356, DSC Onset– 1st Heat, Post cure 4 hrs at 121°C
  • Glass Transition Temp, Tg, ASTM E1356, DSC Onset– 1st Heat, Post cure 8 hrs at 121°C
  • Pot Life, ASTM D2471, 1/2" bead
  • Pot Life, ASTM D2471
  • Shelf Life, resin
  • Shelf Life, hardener
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.