Features: Chemical Resistant; Good Electrical Properties; Good Strength
Test specimen molding conditions: Stock temperature, 315-345°C; Mold temperature, 135°C
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic