MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Phillips 66 Ramar® Diesel XDO SAE Grade 40
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Ramar Diesel XDO is a high-quality, zinc-free, heavy-duty diesel engine oil designed for use in all 2-stroke cycle and 4-stroke cycle railroad locomotive diesel engines. It also is recommended for use in railroad-type diesel engines used in marine service or in stationary service for power generation. It is formulated with a new technology, reduced ash (9 TBN) additive package that is particularly recommended for use in modern EMD and GE power units running on low or ultra-low sulfur diesel fuel. Ramar Diesel XDO is formulated with an advanced additive technology that provides improved oxidative stability, soot dispersancy and wear protection for use in the newer, low exhaust emissions, low oil consumption railroad diesel engines. It has excellent oxidation resistance, high dispersancy and improved TBN retention to protect against deposit formation and help maintain engine cleanliness, even in extended drain or severe service intervals. It provides excellent wear protection and is non-corrosive to yellow metals. The additive package is zinc-free to protect silver bearings and bushings found in older EMD diesel engines, and is non-chlorinated to permit easier recycling or disposal of used oil. Ramar Diesel XDO meets or exceeds the performance requirements of the LMOA Generation 5 and GE Generation 4 Long Life railroad diesel engine oil standards. The low-SAPS formulation is designed for use in diesel engines operating on low or ultra-low sulfur diesel fuel, and also is compatible with the future exhaust aftertreatment technologies under development for use in these engines.

Applications:

  • All 2-stroke cycle and 4-stroke cycle railroad locomotive diesel engines, including newer, low exhaust emissions power units
  • Railroad-type diesel engines used in marine service
  • Railroad-type diesel engines used in stationary service for power generation or offshore drilling equipment
Ramar Diesel XDO is recommended for use in locomotive diesel engines manufactured by:
  • ALCO Engine Division of White Industrial Power, Inc.
  • Baldwin-Lima-Hamilton
  • Cleveland Engine Division of General Motors
  • Electro-Motive Diesel (EMD)
  • Fairbanks Morse
  • General Electric Company
Features/Benefits:
  • New technology, reduced ash (9 TBN) additive package for modern railroad locomotive diesel engines
  • High dispersancy-detergency to protect against sludge and varnish formation
  • Improved TBN retention for extra protection in longer or more severe service intervals
  • Helps keep engines clean and extend oil filter life
  • Minimizes port blocking in 2-stroke cycle engines
  • Protects against rust and corrosion
  • Non-corrosive to silver engine components in older EMD engines
  • Non-chlorinated additive system for easier recycling or disposal of used oil
  • Low-SAPS formulation for compatibility with future exhaust after-treatment technologies
Formerly sold under the 76 Lubricant brand before the manufacturer's product line consolidation.

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, ASTM D874, Sulfated
  • ASTM Color, ASTM D1500
  • Total Base Number, ASTM D2896
  • Pour Point
  • Flash Point, COC
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.