MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Cosmic Plastics ID-40 Orlon Filled Diallyl Iso-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP)

Material Notes: Description: Cosmic ID-40 is an orlon filled, general purpose diallyl ortho phthalate molding compound which is supplied in a granular form. It molds easily in standard compression or transfer equipment.

Features: It has excellent electrical properties and is unaffected by prolonged exposure to elevated temperature and 100% humidity. It is also resistant to solvents, acids, and alkalies. It has good flexural, compressive and tensile strength, and excellent post-mold shrinkage when compared to other orlon molding compounds.

Applications: High resistance to impact and shock makes it an excellent material for terminal and printed circuit boards, connectors, or other applications requiring impact and/or shock tolerance.

Information provided by Cosmic Plastics Inc

Vendors:
Available Properties
  • Density
  • Bulk Factor
  • Water Absorption
  • Linear Mold Shrinkage
  • Tensile Strength at Break
  • Flexural Strength
  • Compressive Strength
  • Izod Impact, Notched
  • Volume Resistivity
  • Volume Resistivity, 100% RH
  • Surface Resistance
  • Surface Resistance, 100% RH
  • Dielectric Constant, Dry
  • Dielectric Constant, Dry
  • Dielectric Constant, Wet
  • Dielectric Constant, Wet
  • Dielectric Strength, Wet, step by step
  • Dielectric Strength, Dry, step by step
  • Dielectric Breakdown, Wet, step by step
  • Dielectric Breakdown, Dry, step by step
  • Dissipation Factor, Dry
  • Dissipation Factor, Wet
  • Dissipation Factor, Dry
  • Dissipation Factor, Wet
  • Arc Resistance
  • CTE, linear
  • Heat Distortion Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.