MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Teijin Twaron® Standard Modulus, High Elongation Aramid Yarn
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: Twaron® para-aramid has excellent mechanical properties, chemical resistance, durability, and thermal stability. The characteristics of Twaron® are the result of a 100% paracrystalline structure with molecular chains preferentially oriented along the yarn filament axis.

Twaron® filament yarn uses include optical fiber cables, hoses, tires, rubber products, ballistic protection, protective clothing, ropes and cables, composites and belts. Twaron® filament yarn is available in yellow (and dyed black in certain yarn types).

Information provided by Teijin Aramid B.V.

Vendors:
Available Properties
  • Density
  • Moisture Absorption
  • Elongation at Break
  • Modulus of Elasticity
  • Tenacity
  • Maximum Service Temperature, Air, strength retention limit
  • Minimum Service Temperature, Air, mechanical properties retained
  • Decomposition Temperature
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.