MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE™ 2000EZ is a high-heat PC/ABS resin delivering optimized performance for automotive interior component applications.

Benefits:

  • Easy flow, reduced scrap, and faster cycle times, while enabling thin wall part design for mass reduction
  • High-impact strength even at low temperature
  • High Heat resistance for demanding automotive interior components
  • Consistent natural white color produces high quality part appearance when used with color concentrates (self coloring) or Trinseo Color Masterbatch Technology
  • Low odor & VOC to meet all global Automotive OEM specifications
Applications:
  • Mid (floor) consoles
  • Instrument Panel components
  • Door panel trim
  • Pillars
  • Storage/load floors/glove box
Automotive Specifications:
  • 3M 11-0003-5762-1
  • CHRYSLER MS-DB-195 CPN2967
  • CHRYSLER MS-DB-195 CPN3401
  • CHRYSLER MS-DB-195 CPN4598
  • DAIMLER DBL 5404.29
  • GM GMW155819-ABS+PC-T3
  • RNPO AS33
  • TOYOTA TSM 5526G-2
  • VOLKSWAGEN TL 522 31-A
  • BMW GS 93016
  • CHRYSLER MS-DB-195 CPN3159
  • CHRYSLER MS-DB-195 CPN3408
  • DAIMLER DBL 5404.28
  • FORD WSS-M4D585-C1
  • GM GMW15581P-ABS+PC-T6
  • TESLA TM-1003 10/20
  • VOLKSWAGEN TL 522-31
  • VOLKSWAGEN TL 522-31-B

Information provided by Trinseo.

Vendors:
Available Properties
  • Density, ISO 1183/B
  • Apparent Bulk Density, ISO 60
  • Linear Mold Shrinkage
  • Melt Flow, ISO 1133
  • Spiral Flow, Melt Temp: 260°C, Mold Temp: 60°C, Injection Pressure: 1.8E+3 bar
  • Tensile Strength, Yield, ISO 527-2/50
  • Elongation at Break, ISO 527-2/50
  • Tensile Modulus, ISO 527-2, Injection Molded, 1 mm/min
  • Flexural Modulus, ISO 178, 2.0 mm/min
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • Vicat Softening Point, ISO 306/B50
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.