MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Danquinsa MORCHEM UD 5152HR Polyurethane dispersion
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: MORCHEM UD 5152HR is a application ready, aqueous, aliphatic structured polyester urethane dispersion. This fast crystalline polyurethane dispersion distinguish itself by its extreme good adhesion on polyester and polyether foam as well as through its high adhesive strength on polyester fabrics. The aliphatic based PU dispersion is acting for the production of shoe adhesives as well as for the production of textile and leather finishes.

Application: MORCHEM UD 5152HR is applied to serve as a basic raw material by the production of aqueous 1- and 2-component adhesives. Adhesives and adhesive coatings which were produced with MORCHEM UD 5152HR are especially good suitable for:

  • Textile lamination
  • Coating of casings and profiles
  • Lamination of thermoplastic foils with wooden materials as for instance by membrane press application
  • Deep-draw and press lamination application for the automotive industry.
  • Shoe soles- and shoe shank fitting
  • Lamination of split leather and plastic foils.
We recommend, for the processing of 2- component adhesives, the application of the cross link agent DANCURE 101.

Information provided by Danquinsa GMBH

Vendors:
Available Properties
  • Solids Content
  • pH
  • Viscosity
  • Storage Temperature
  • Tensile Strength, DIN 53.504
  • Elongation at Break, DIN 53.504
  • 100% Modulus, DIN 53.504
  • 300% Modulus, DIN 53.504
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.