MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grades. This can, of course, raise the cost of toolmaking. Due to the very carefully balanced alloying and the powder metallurgical manufacturing route, Uddeholm Vanadis 6 has a similar hardening procedure as the common cold work tool steel. In order to reduce the amount of retained austenite and to optimize the abrasive wear resistance high temperature tempering is recommended. One very big advantage with Uddeholm Vanadis 6 is that the dimensional stability after hardening and tempering is much better than for conventionally produced cold work steel and HSS used for cold work. This also means that Uddeholm Vanadis 6 is a tool steel which is very suitable for CVD and PVD coating

Vanadis 6 is characterized by:

  • Very high abrasive-adhesive wear resistance
  • High compressive strength
  • Good toughness
  • Very good dimensional stability at heat treatment and in service
  • Very good through-hardening properties
  • Good resistance to tempering back
  • High cleanliness

Vendors:
Available Properties
  • Density, hardness of 60 HRC
  • Hardness, Brinell, Soft annealed
  • Hardness, Rockwell C, Hardened and tempered
  • Modulus of Elasticity, (hardness of 60 HRC)
  • Modulus of Elasticity, hardness of 60 HRC
  • Modulus of Elasticity, hardness of 60 HRC
  • Compressive Yield Strength, 0.2%, hardness of 60 HRC, tempered at 977°F 2 + 2h.
  • Compressive Yield Strength, 0.2%, hardness of 62 HRC, tempered at 977°F 2 + 2h.
  • Compressive Yield Strength, 0.2%, hardness of 64 HRC, tempered at 977°F 2 + 2h.
  • Impact Test, hardness of 62 HRC
  • CTE, linear, hardness of 60 HRC
  • CTE, linear, hardness of 60 HRC
  • Specific Heat Capacity, hardness of 60 HRC
  • Thermal Conductivity, hardness of 60 HRC
  • Thermal Conductivity, hardness of 60 HRC
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.