MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Sandvik 13RM19 Stainless Spring Wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Sandvik 13RM19 combines high mechanical strength with a non-magnetic structure. This combination of properties has previously been found mainly in expensive Co-Ni-base or Cu-Be-alloys. The steel has very good corrosion resistance comparable to that of AISI 302.

Sandvik 13RM19 is characterized by:

  • non-magnetic structure in all conditions
  • very high mechanical strength in the cold drawn condition. The strength can be further increased without any effect on the non-magnetic structure by a simple tempering operation
  • high elastic limit and energy storing capacity in the cold drawn and tempered condition

Sandvik 13RM19 also possesses good fatigue properties and excellent ductility, which makes it a most suitable choice for springs and other high strength applications where ferromagnetic materials cannot be used.

Service temperature: up to 250°C (480°F)

Information provided by Sandvik

EN 1.4369

Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Modulus of Elasticity, as delivered
  • Modulus of Elasticity, as tempered
  • Poissons Ratio, Calculated
  • Shear Modulus, as received
  • Shear Modulus, as tempered
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Maximum Service Temperature, Air
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Nickel, Ni
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.