- Density, Average value: 1.30 g/cc Grade Count:286
- Density, Average value: 1.09 g/cc Grade Count:16
- Water Absorption, Average value: 2.01 % Grade Count:17
- Moisture Absorption at Equilibrium, Average value: 0.244 % Grade Count:11
- Moisture Absorption at Equilibrium, Average value: 0.950 % Grade Count:1
- Moisture Absorption at Equilibrium, Average value: 0.950 % Grade Count:1
- Additive Loading, Average value: 20.0 % Grade Count:14
- Moisture Vapor Transmission, Average value: 11.5 cc-mm/m²-24hr-atm Grade Count:4
- Water Vapor Transmission, Average value: 103 g/m²/day Grade Count:8
- Oxygen Transmission, Average value: 20.3 cc-mm/m²-24hr-atm Grade Count:4
- Oxygen Transmission Rate, Average value: 889 cc/m²/day Grade Count:7
- Nitrogen Transmission, Average value: 4.74 cc-mm/m²-24hr-atm Grade Count:4
- Carbon Dioxide Transmission, Average value: 94.0 cc-mm/m²-24hr-atm Grade Count:4
- Maximum Moisture Content, Average value: 0.0320 Grade Count:5
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse, Average value: 0.00369 cm/cm Grade Count:9
- Melt Flow, Average value: 12.8 g/10 min Grade Count:232
- Hardness, Rockwell R, Average value: 105 Grade Count:20
- Hardness, Shore A, Average value: 76.8 Grade Count:8
- Hardness, Shore D, Average value: 69.0 Grade Count:19
- Ball Indentation Hardness, Average value: 131 MPa Grade Count:4
- Tensile Strength, Ultimate, Average value: 57.3 MPa Grade Count:191
- Tensile Strength, Ultimate, Average value: 27.8 MPa Grade Count:2
- Film Tensile Strength at Yield, MD, Average value: 30.5 MPa Grade Count:13
- Film Tensile Strength at Yield, TD, Average value: 26.5 MPa Grade Count:13
- Tensile Strength, Yield, Average value: 45.2 MPa Grade Count:78
- Tensile Strength, Yield, Average value: 47.8 MPa Grade Count:2
- Film Elongation at Break, MD, Average value: 489 % Grade Count:48
- Film Elongation at Break, TD, Average value: 554 % Grade Count:48
- Elongation at Break, Average value: 69.4 % Grade Count:256
- Elongation at Break, Average value: 41.3 % Grade Count:2
- Elongation at Yield, Average value: 26.7 % Grade Count:55
- Elongation at Yield, Average value: 2.00 % Grade Count:2
- Modulus of Elasticity, Average value: 2.35 GPa Grade Count:226
- Modulus of Elasticity, Average value: 5.92 GPa Grade Count:2
- Modulus of Elasticity, Average value: 5.92 GPa Grade Count:1
- Modulus of Elasticity, Average value: 5.92 GPa Grade Count:1
- Tenacity, Average value: 0.307 N/tex Grade Count:11
- Flexural Yield Strength, Average value: 77.4 MPa Grade Count:125
- Flexural Yield Strength, Average value: 85.0 MPa Grade Count:2
- Flexural Modulus, Average value: 3.38 GPa Grade Count:146
- Flexural Modulus, Average value: 3.28 GPa Grade Count:2
- Flexural Strain at Break, Average value: 3.49 % Grade Count:12
- Secant Modulus, Average value: 0.354 GPa Grade Count:5
- Secant Modulus, MD, Average value: 3.35 GPa Grade Count:3
- Secant Modulus, TD, Average value: 3.85 GPa Grade Count:3
- Izod Impact, Notched, Average value: 1.39 J/cm Grade Count:84
- Izod Impact, Notched, Average value: 0.929 J/cm Grade Count:16
- Izod Impact, Unnotched, Average value: 5.87 J/cm Grade Count:38
- Izod Impact, Unnotched, Grade Count:1
- Izod Impact, Notched (ISO), Average value: 11.9 kJ/m² Grade Count:20
- Izod Impact, Notched (ISO), Average value: 17.9 kJ/m² Grade Count:7
- Izod Impact, Unnotched (ISO), Average value: 20.1 kJ/m² Grade Count:11
- Izod Impact, Unnotched (ISO), Average value: 64.5 kJ/m² Grade Count:2
- Charpy Impact Unnotched, Average value: 2.56 J/cm² Grade Count:92
- Charpy Impact Unnotched, Grade Count:1
- Charpy Impact, Notched, Average value: 0.766 J/cm² Grade Count:76
- Charpy Impact, Notched, Average value: 4.60 J/cm² Grade Count:1
- Coefficient of Friction, Average value: 0.195 Grade Count:11
- Coefficient of Friction, Static, Average value: 0.266 Grade Count:11
- Tear Strength, Average value: 80.3 kN/m Grade Count:12
- Elmendorf Tear Strength MD, Average value: 312 g Grade Count:6
- Elmendorf Tear Strength TD, Average value: 323 g Grade Count:6
- Elmendorf Tear Strength, MD, Average value: 0.426 g/micron Grade Count:16
- Elmendorf Tear Strength, TD, Average value: 0.510 g/micron Grade Count:16
- Dart Drop Total Energy, Average value: 347 J/cm Grade Count:3
- Dart Drop Test, Average value: 199 g Grade Count:10
- Film Tensile Strength at Break, MD, Average value: 29.8 MPa Grade Count:41
- Film Tensile Strength at Break, TD, Average value: 31.1 MPa Grade Count:41
- Electrical Resistivity, Average value: 6.67e+14 ohm-cm Grade Count:6
- Surface Resistance, Average value: 6.67e+14 ohm Grade Count:6
- Dielectric Constant, Average value: 2.29 Grade Count:3
- Dissipation Factor, Average value: 0.00750 Grade Count:3
- CTE, linear, Average value: 114 µm/m-°C Grade Count:3
- Thermal Conductivity, Average value: 0.0439 W/m-K Grade Count:4
- Melting Point, Average value: 154 °C Grade Count:124
- Maximum Service Temperature, Air, Average value: 175 °C Grade Count:30
- Deflection Temperature at 0.46 MPa (66 psi), Average value: 86.1 °C Grade Count:140
- Deflection Temperature at 1.8 MPa (264 psi), Average value: 82.6 °C Grade Count:53
- Vicat Softening Point, Average value: 85.5 °C Grade Count:64
- Glass Transition Temp, Tg, Average value: 57.1 °C Grade Count:65
- Flammability, UL94, Grade Count:20
- Haze, Average value: 30.8 % Grade Count:7
- Gloss, Average value: 90.0 % Grade Count:4
- Transmission, Visible, Average value: 90.0 % Grade Count:13
- Processing Temperature, Average value: 184 °C Grade Count:71
- Nozzle Temperature, Average value: 196 °C Grade Count:61
- Adapter Temperature, Average value: 203 °C Grade Count:12
- Die Temperature, Average value: 178 °C Grade Count:45
- Melt Temperature, Average value: 182 °C Grade Count:139
- Mold Temperature, Average value: 64.1 °C Grade Count:120
- Injection Velocity, Average value: 36.5 mm/sec Grade Count:15
- Drying Temperature, Average value: 69.0 °C Grade Count:154
- Drying Temperature, Average value: 56.3 °C Grade Count:4
- Moisture Content, Average value: 0.211 % Grade Count:87
- Moisture Content, Average value: 0.192 % Grade Count:13
- Dew Point, Average value: -38.1 °C Grade Count:99
- Drying Air Flow Rate, Average value: 14.2 l/min Grade Count:24
- Injection Pressure, Average value: 81.4 MPa Grade Count:35
|
| | |