Moplen RP215MY B is a polypropylene random copolymer designed for casting film, without anti-block and slip agent. Moplen RP215MY B is suitable for food contact. Availability: Asia-Pacific Application: Food Packaging Film Market: Flexible Packaging Processing Method: Cast Film; Extrusion Flat-die Attribute: Random Copolymer Information provided by LyondellBasell. |