MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil 111 Mobilux EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the soap thickener at extremely high rotating speeds, ensuring effective lubrication and protection against wear even in heavily loaded misaligned gear couplings. Mobilux EP 111 is a lithium hydroxystearate grease formulated with an extremely heavy, viscous mineral base oil. Mobilux EP 111 also contains an oil soluble molybdenum additive, as well as a very effective corrosion inhibitor. It is an NLGI 1 Grade grease. In addition to being used in a wide range of coupling designs, Mobilux EP 111 can also be used in low-speed open gearing and plain bearings. This grease has shown excellent performance and protection in a wide variety of coupling applications covering a broad range of industries. Based on its longstanding performance capabilities, this grease has become the product of choice for many users.

Mobilux EP 111 is recommended for all types of heavily loaded lubricated couplings. Mobilux EP 111 has a recommended operating temperature range of -10 to 120º C. Mobilux EP 111 has performed very well in the following applications: Gear and grid couplings; Spring and slipper joint couplings; Spindle (gear) and chain couplings; Low speed open gears and plain bearings

Key Words: NLGI Grade 1
Vendors:
Available Properties
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear, ASTM D2266
  • Penetration, ASTM D217, Worked, 25°C
  • Timken Test
  • Dropping Point, ASTM D2265
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.