MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
GEHR Plastics MEDI-GEHR® PPSU MG
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Polyphenylenesulfone is an amorphous material, with improved impact and hydrolysis resistance compared to PSU. This amber-colored, transparent material is usually used in a black color, which is why we only offer it in this color version so far. The usual operating temperature is approx. +170 °C. The extremely high notch impact strength remains also after a heat aging.

Features: High strength and rigidity; Very high impact strength (also at low temperatures); Very good dimensional stability; Very high chemical resistance; High resistance to many kinds of radiation; Very good sterilizing capability; Lower chemical resistance than comparable semicrystalline materials

Typical Applications: Instrument handles; Instruments for microinvasive surgery; Sterilization cassettes; Analysis technology; In vitro diagnostics; Food industry; Pump wheels; Valves

Information provided by GEHR Plastics, Inc.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Water Absorption, ISO 62
  • Moisture Absorption, ISO 62
  • Hardness, Shore D, ISO 868
  • Ball Indentation Hardness, ISO 2039
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Strength, ISO 178
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, ISO 11359
  • Thermal Conductivity, ISO 22007-4
  • Melting Point, ISO 3146
  • Maximum Service Temperature, Air, UL746B
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Minimum Service Temperature, Air, UL746B
  • Glass Transition Temp, Tg, ISO 3146
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GEHR Plastics Inc

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.