MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
CHT Group True Skin® 10 10 Shore A, Clear Addition Cure Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: True Skin® 10 is a translucent, two-component, room temperature, addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. In addition, the material is pigmentable and has a low viscosity that allows for easy processing.

Key Features:

  • Low viscosity
  • Translucent for ease of pigmentation
  • Excellent flexibility
  • Can be diluted with dimethyl fluid with minimal bleed
Main Applications:
  • Special effects
  • Animatronics
  • Prosthetics
  • Skin replication
  • Applications where pigmentation is required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors:
Available Properties
  • Specific Gravity, Uncatalyzed, True Skin® 10 A
  • Specific Gravity, Uncatalyzed, True Skin® 10 B
  • Viscosity, Uncatalyzed, True Skin® 10 A
  • Viscosity, Uncatalyzed, True Skin® 10 B
  • Viscosity, Catalyzed
  • Linear Mold Shrinkage, Cured 3 days at 25°C
  • Hardness, Shore A, Cured 3 days at 25°C
  • Tensile Strength, Cured 3 days at 25°C
  • Elongation at Break, Cured 3 days at 25°C
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dry Time, Catalyzed, Demold
  • Cure Time
  • Pot Life, Catalyzed
  • Gel Time, Catalyzed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.