ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2a, allowing for use in packing or holding food during cooking when used unmodified and according to good manufacturing practices for food contact application. Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |