MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Röhm ACRYLITE® Soundstop GS CC Cast Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: ACRYLITE® Soundstop GS CC is a highly transparent grade of cast acrylic with embedded polyamide threads. In the event of breakage due to an accident, these threads retain any sheet fragments and prevent them from falling down.

Properties: In addition to the well-known and proven properties of ACRYLITE® such as:

  • excellent light transmission and brilliance
  • extremely high weather resistance
  • high surface hardness
  • low weight – half the weight of glass
  • 11times the impact strength of glass
  • 100% recyclability,
ACRYLITE® Soundstop GS CC offers the following special features:
  • Superior safety. ACRYLITE® Soundstop GS CC panels meet the fragment prevention requirements of EN-1794-2.
  • Embedded black filaments reduce the odds of bird collision.
  • Superior sound reduction rating (STC) of32 dB or higher by ASTM E 90.
  • Lightweight applications for noise barriers
  • Complies with European noise barrier regulations railways (including high speed rail) RIL 804.5501.
  • ACRYLITE® Soundstop GS CC is availablein transparent colors.
Applications: These properties make ACRYLITE® Soundstop GS CC especially suitable for
  • noise control on highway and railway bridges.
  • wind barriers on bridges

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors:
Available Properties
  • Density, ASTM D729
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus
  • Compressive Yield Strength, ASTM D695
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003
  • Haze, ASTM D1003, Weathered 5 years
  • Yellow Index, ASTM D1925
  • Yellow Index, ASTM D1925, Weathered 5 years
  • Transmission, Visible, ASTM D1003
  • Transmission, Visible, ASTM D1003, Weathered 5 years
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Röhm GmbH , former product of Evonik Corporation; Evonik Cyro

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.