MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Dow Dow™ DMDA-8904 HEALTH+™ HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow HDPE DMDA-8904 HEALTH+™ is a narrow molecular weight distribution high density copolymer designed to offer excellent stiffness, environmental stress crack resistance, and good moldability. The resin is suitable for injection-molded medical devices such as IV kit components and respiratory care. Films can also be cast from this product yielding good barrier and stiffness.
Main Characteristics:
  • Excellent stiffness
  • Excellent stress crack resistance
  • Good processability
  • High gloss parts
Complies with: US FDA 21 CFR 177.1520©3.2a; EU, No 10/2011; Canadian HPFB No Objection; USP XXI Class VI; Drug Master File Listing. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; EU No 10/2011; FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; USP XXI Class VI

Form: Pellets

Processing Method: Injection Molding

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • ESCR 100% Igepal®, ASTM D1693, F50, Molded and tested in accordance with ASTM D4976
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Film Tensile Strength at Yield, MD, ASTM D882, Cast Film
  • Film Tensile Strength at Yield, TD, ASTM D882, Cast Film
  • Tensile Strength, Yield, ASTM D638
  • Film Elongation at Break, MD, ASTM D882, Cast Film
  • Film Elongation at Break, TD, ASTM D882, Cast Film
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Modulus, ASTM D790B
  • 2% Secant Modulus, ASTM D882, MD, Cast Film
  • Tensile Impact Strength, ASTM D1822, Type S, Molded and tested in accordance with ASTM D4976
  • Elmendorf Tear Strength MD, ASTM D1922, Cast Film
  • Elmendorf Tear Strength TD, ASTM D1922, Cast Film
  • Dart Drop Test, ASTM D1709A, Cast Film
  • Film Tensile Strength at Break, MD, ASTM D882, Cast Film
  • Film Tensile Strength at Break, TD, ASTM D882, Cast Film
  • Melting Point
  • Crystallization Temperature
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746, Molded and tested in accordance with ASTM D4976
  • Haze, ASTM D1003, Cast Film
  • Gloss, ASTM D2457, 45°, Cast Film
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Flame Retardant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.