MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Meldin Supplier
DuPont Mobility and Materials Vespel® SP-202 Conductive Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Vespel® SP-202 has the combination of capabilities that meet these demanding applications.
  • Electrostatic charge removal. Vespel® SP-202 is a conductive plastic grade with surface and volume resistivity values in the range of 10–1 to 101 (ohm, ohm-cm).
  • Vespel® SP-202 has the thermal resistance to maintain tolerances in high heat applications and through multiple thermal cycles.
  • Lower wear rates on contact surfaces generate longer part life and cleaner environments.
  • Vespel® SP-202 can be machined to tight tolerances with relative ease.
Benefits:
  • Although material cost is higher than some engineering plastics, lower scrap rates and machining cost may yield offsetting savings during the fabrication process.
  • Low wear rates will provide consistent positioning and long part life resulting in high production utility and low maintenance cost.
  • Low particle generation will keep operating environments clean.
  • Properly grounded components will not hold a charge preventing the attraction of dust and other charged particles.

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Rockwell E, ASTM D785, Parallel
  • Hardness, Rockwell E, ASTM D785, Perpendicular
  • Tensile Strength at Break, ASTM D638, Parallel
  • Tensile Strength at Break, ASTM D638, Perpendicular
  • Tensile Strength at Break, ASTM D638, Parallel
  • Tensile Strength at Break, ASTM D638, Perpendicular
  • Elongation at Break, ASTM D638, Parallel
  • Elongation at Break, ASTM D638, Parallel
  • Elongation at Break, ASTM D638, Perpendicular
  • Elongation at Break, ASTM D638, Perpendicular
  • Tensile Modulus, ASTM D638, Parallel
  • Tensile Modulus, ASTM D638, Perpendicular
  • Tensile Modulus, ASTM D638, Parallel
  • Tensile Modulus, ASTM D638, Perpendicular
  • Flexural Strength, ASTM D790, Perpendicular
  • Flexural Strength, ASTM D790, Parallel
  • Flexural Strength, ASTM D790, Perpendicular
  • Flexural Strength, ASTM D790, Parallel
  • Flexural Modulus, ASTM D790, Perpendicular
  • Flexural Modulus, ASTM D790, Parallel
  • Flexural Modulus, ASTM D790, Perpendicular
  • Flexural Modulus, ASTM D790, Parallel
  • Compressive Strain at Break, ASTM D695, Parallel
  • Compressive Strain at Break, ASTM D695, Parallel
  • Compressive Strain at Break, ASTM D695, Perpendicular
  • Compressive Strain at Break, ASTM D695, Perpendicular
  • Compressive Strength, ASTM D695, Perpendicular
  • Compressive Strength, ASTM D695, Parallel
  • Compressive Strength, ASTM D695, Perpendicular
  • Compressive Strength, ASTM D695, Parallel
  • Volume Resistivity, ASTM D991, Perpendicular
  • Volume Resistivity, ASTM D991, Parallel
  • Surface Resistance, ASTM D991, Parallel
  • Surface Resistance, ASTM D991, Perpendicular
  • CTE, linear, ASTM E831, Perpendicular
  • CTE, linear, ASTM E831, Parallel
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.