MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Teknor Apex Monprene® RG-20170 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-20100 series is group of high performance thermoplastic elastomer specifically designed for extruded regulated applications including food contact, toys and children’s products. Monprene RG-20170 is a low density, Medium hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: BPA Free, Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Low Flow; Low Density; Low Specific Gravity; Lubricated; Medium Hardness; No Animal Derived Components; Slip; Without Fillers

Uses: Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Service Applications; Kitchenware; Lids; Non-specific Food Applications; Rubber Replacement; Toys

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ISO 868, Injection Molded
  • Hardness, Shore A, ISO 868, Injection Molded
  • Tensile Strength at Break, ASTM D412, 20 in/min, Flow
  • Tensile Strength at Break, ASTM D412, 20 in/min, Across Flow
  • Tensile Stress at Strain, ASTM D412, 20 in/min, Across Flow
  • Tensile Stress at Strain, ASTM D412, 20 in/min, Across Flow
  • Tensile Stress at Strain, ASTM D412, 20 in/min, Flow
  • Tensile Stress at Strain, ASTM D412, 20 in/min, Flow
  • Elongation at Break, ASTM D412, 20 in/min, Flow
  • Elongation at Break, ASTM D412, 20 in/min, Across Flow
  • Tear Strength, ISO 34-1, Method Ba, Angle (Unnicked), 20 in/min, Across Flow
  • Tear Strength, ISO 34-1, Method Ba, Angle (Unnicked), 20 in/min, Flow
  • Compression Set, ISO 815, Type A
  • Compression Set, ISO 815, Type A
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Die Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.