MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Elkem (Bluestar Silicones) SILBIONE® LSR 4301 Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Description: SILBIONE® Liquid Silicone Rubbers (LSRs) are two-component platinum-catalyzed silicone elastomers designed for liquid injection molding healthcare and medical devices, including applications of less than 30 day implantation in the human body. Available in 01 to 25 durometer Shore A, Bluestar Silicones’ SILBIONE® LSRs offer the distinctive advantages of easy processing and easy release combined with high performance physical properties. Designed specifically for healthcare applications, SILBIONE® LSRs meet or exceed testing requirements of United States Pharmacopoeia (USP) Class VI. Biocompatibility testing addresses the categories of evaluation for cytotoxicity, skin sensitization and skin irritation specified in ISO 10993 for device use of less than 30 days duration. See Table 2.

Applications: The easy processing and high performance physical properties of the SILBIONE® LSRs make them suitable for a broad range of applications including

  • Fabrication of healthcare and medical devices, including less than 30 day implantation
  • Skin contact parts like liners
  • Balloons
  • Orthopedic Insoles and cushioning applications
  • Prosthetic liners
  • Rollers
Features:
  • Easy processing and convenient 1:1 mix ratio
  • Excellent mold release for shorter cycle times
  • Superior clarity
  • High performance physicals – high tear and elongation; can be molded into thin-walled parts
  • Rebound resilience characteristics – cushioning and non-tacky
  • Rapid cure at elevated temperatures
  • Can be post-cured, but post cure is not necessary to achieve desired physicals
  • Easily pigmented
  • Soft, skin-like feel when molded

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity, TP 013
  • Viscosity, TP 005
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240, Press Cured, 5 min, 177°C
  • Hardness, Shore OO, ASTM D2240, Press Cured, 5 min, 177°C
  • Tensile Strength, ASTM D412, Press Cured, 5 min, 177°C
  • Elongation at Break, ASTM D412, Press Cured, 5 min, 177°C
  • 100% Modulus, ASTM D412, Press Cured, 5 min, 177°C
  • Tear Strength, ASTM D624, Die B, Press Cured, 5 min, 177°C
  • Shelf Life
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.