MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP21TDC-2AO Flexibilized, Thermally Conductive Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Highly flexible
  • Serviceable from 4K to +250°F
  • Excellent impact resistance
  • Thermally conductive/electrically insulative
  • High peel strength properties
  • Ambient temperature cures
Product Description: Master Bond Polymer System EP21TDC 2AO is a two component highly flexible epoxy resin compound for high performance bonding sealing, coating and encapsulation. It is formulated to cure fully at ambient temperatures or more quickly at elevated temperatures with an easy to use one to three mixing ratio by weight. The cured compound exhibits a high elongation (greater than 25%), truly exceptional for a thermally conductive epoxy. After mixing EP21TDC-2AO generates a very low exotherm, which allows for a long working life. This epoxy resin compound exhibits good tensile shear and peel strength for bonding and sealing many different substrates including metals, glass, ceramics, vulcanized rubber and many plastics. The cured epoxy is an excellent electrical insulator with superior chemical resistance to water, fuels and many solvents. Most noteworthy is its ability to withstand thermal shock, thermal cycling and mechanical shock. Featuring a service temperature range of 4K to 250°F, it has been successfully employed in a number of cryogenic applications. Master Bond EP21TDC-2AO is an exceptionally versatile system that offers the structural benefits of an epoxy, yet incorporates flexibility and impressive thermal conductivity. It is widely used in the electronic, electro-optical and related industries. The color of Part A is gray; Part B is offwhite.

Product Advantages:

  • Convenient mixing: non-critical one to three weight ratio
  • Easy application: product spreads evenly and Smoothly
  • 100% reactive, no solvents or volatiles emitted during cure or in service
  • Versatile cure schedules; ambient temperature cures or faster, elevated temperature cures
  • High peel strength and elongation
  • Excellent flexibility; exceptional thermal shock and chemical resistance
  • Superior bonding properties to similar and dissimilar substrates; superb impact resistance
  • High thermal conductivity combined with good electrical insulation properties
  • Cryogenically serviceable down to 4K

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Peel Strength
  • Volume Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.