MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco Texcool® P 200
Categories: Fluid

Material Notes: In service Texaco Texcool P 200 provides:
  • Silicate free
  • Excellent heat transfer properties
  • Superior corrosion protection for brass, copper, solder, steel and cast iron
  • Nitrite-free, amine-free
  • Mixes readily with clean tap water
  • 100% biodegradable in its pure unused form

Texaco Texcool P 200 is a superior quality, single phase, propylene glycol (USP) based product. It is a silicate free coolant designed for use in the immersion or spray freezing equipment of packaged poultry or wrapped meat under the Federal Meat and Poultry Products Inspection Program. Texaco Texcool P 200 must be used in a manner which prevents direct or indirect contamination of edible products in official establishments operating under the Federal Meat and Poultry Products Inspection Program.

Texaco Texcool P 200 is a single phase, propylene glycol (USP) based product blended with a premium quality additive package. It is a silicate free coolant designed and approved for use in immersion or spray freezing equipment of packaged poultry or meat under the Federal Meat and Poultry Products Inspection Program. Texaco Texcool P 200 should not be used for automotive or nonstationary heavy duty diesel applications. This product provides antifoam properties, and rust and corrosion protection for brass, copper, solder, steel and cast iron. It mixes readily with any clean tap water and is compatible with cooling system filters and supplemental additives.

Texaco Texcool P 200 is free of nitrites and amines.

Texaco Texcool P 200 is an inhibited propylene glycol (USP) based product that is used as an industrial coolant and heat transfer agent. In non-USDA applications, Texaco Texcool P 200 may be used in applications where incidental contact with food is possible. This product is not intended for use as a food component or additive. The inhibitor system is designed to protect brass, copper, solder, steel, cast iron, aluminum, and other metals commonly found in industrial cooling and heating systems. A foam inhibitor is included to minimize foaming tendencies during service.

Extensive laboratory simulated service and actual service tests have proven the effectiveness of Texaco Texcool P 200 coolant in preventing corrosion. Use of Texaco Texcool P 200 coolant for heat transfer applications in place of brine solutions or uninhibited glycol water solutions lowers maintenance costs and improved heat transfer.

Texaco Texcool P 200 meets the requirements of the U.S. Department of Agriculture (USDA) for use in the immersion or spray freezing equipment of packaged poultry or wrapped meat under the Federal Meat and Poultry Products Inspection Program.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 227940; MSDS Number: 10700

Vendors:
Available Properties
  • Specific Gravity, 60/60°C
  • Melting Point, ASTM D1177, 50 vol % Aqueous Solution
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.