MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Phillips 66 Omniguard® XD5 NLGI Grade 0
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Omniguard XD5 is a premium quality, high-performance, extreme pressure (EP) calcium sulfonate grease developed to satisfy the severe lubrication requirements of mining and off-road equipment manufactured by Caterpillar, Terex, Komatsu Dresser, Le Tourneau, P&H and others. It is particularly recommended for use in AC and DC electric-drive haul trucks, cranes, scrapers, shovels and drag lines operating under wet conditions and/or moderate to high temperatures and under heavy loading. Omniguard XD5 is manufactured with high-quality base oils and a non-soap, calcium sulfonate thickener. It is compounded with select additives that provide extreme-pressure and antiwear properties, excellent rust and corrosion protection, and excellent oxidation resistance. It is fortified with 5% molybdenum disulfide(moly) for extra wear protection under heavy or shock loading. Functional polymers provide better adhesion to metal surfaces and enhanced resistance to water washout in wet environments.

Applications:

  • Chassis parts and wheel bearings of mine haul trucks and other off-highway equipment
  • Heavily loaded plain and rolling-element bearings in industrial and mobile equipment where the manufacturer specifies a high-temperature, extreme-pressure grease with 5% moly
Features/Benefit:
  • High dropping point (>550°F)
  • High load-carrying capacity
  • Excellent wear protection
  • Contains 5% moly for extra protection against galling and wear under shock loads
  • Excellent oxidation resistance
  • Excellent resistance to water washout
  • Excellent rust and corrosion protection

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D942, Pressure Drop
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear, ASTM D2266, Scar Diameter
  • Penetration
  • Timken Test, ASTM D2509, OK Load
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.