MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Chesterton 273 Electric Motor Cleaner
Categories: Fluid

Material Notes: Description: Chesterton® 273 Electric Motor Cleaner is a nonflammable, nonconductive and noncorrosive solvent based degreaser. It can be used on operating equipment and electrical systems without concern as to fire hazard. The product instantly cuts through power-robbing grease, dirt grime, tar oil and other materials usually found around electrical equipment, machine ships, manufacturing plants, marine electrical instrumentation and automotive applications. Chesterton 273 Electric Motor Cleaner removes these conductive soils that could otherwise cause dangerous electrical short circuits. Applied at regular intervals together with routine inspection and periodic maintenance, 273 Electric Motor Cleaner will assure continued, high output and prolong the life of electrical equipment.

Features:

  • Nonflammable
  • Nonconductive
  • High Dielectric strength
  • Fast Penetration-High Solvency
  • NSF K2 – registration number 133975 (bulk) and 133976 (aerosol)

Applications: Cleans electrical equipment without harming electrical wiring, rubber, insulation or contact. An excellent degreaser for electric motors, fuse holders, blowers, fans hoists, switches, transformers and cables.

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.