The MC/HE Series is recommended for applications requiring basic medical approvals such as USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11. The series is characterized by combining excellent elasticity with high hardness. The compounds are produced exclusively by a special medical unit and available in translucent colors. Typical applications: - Drip chamber
- Luer lock
- Squeeze bottles
Material advantages:- Adhesion to PP
- DMF listed
- Free of animal base ingredients
- High elasticity
- High stiffness
- KRAIBURG TPE Medical service package (description below)
- Sterilizable (autoclave134 °C, gamma radiation 2x35 kGy, EtO)
- Tested according to USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11
Processing Method: Injection MoldingInformation provided by Kraiburg TPE. A newer data sheet is available in MatWeb. |